전기아연도금강판
 

Class Type Coating
Structure
Quality Features Use
Corrosion Resistance Paintability Fingerprint Resistance Weldability Conductive
Phosphating PL Phosphate coating of 1~3g/㎡ for improvement of paintability Painting
Chromating General Use(CL) Chromating of 5~15mg/㎡for improvement of corrosion resistance. General Uses
Special Use (CM) (CH) Using CM(30~60mg/㎡) CH(80~160mg/㎡) to increase Cr coating weight for the purpose of strengthen corrosion resistance much than general Cr Inner Plate of Home Appliances
Lubricating Steel Plate General Cr Lubricating (LD) Available for machining without press oil because it is coated by lubricating resin after Cr treatment Cr:5~15mg/㎡ Resin:0.6~1.0um Motor Case, CassetteVTR Desk, Printer panel, Home appliance panel
After Cr Lubricating (LH) Available for machining without press oil because it is coated by lubricating resin after Cr treatment Cr:30~50mg/㎡ Resin:0.6~1.0um
Fingerprint Resistance Treatment General Thin Film Treatment   (AD) Thin film is treated on a resin layer in order to improve conductivity compared to thick film steel. (0.5~1.1um) Computer case, Cassette VTR desk
Special Thin Film Treatment (AH) (AM) After Cr treatment for high corrosion resistance and conductivity (AH:Cr30~60mg/㎡, AM:Cr80~160mg/㎡) Then, thin film treatment on a resin layer (0.5~1.1um) Cassette VTR Desk, Home appliance panel
1. ● Very Excellent, ◎ Excellent, ○ Good
2. Coating Structure of Lubricating Steel Plate and Fingerprint Resistant Products
3. CM,AH: Manufactured in Pohang ,CH,AM: Manufactured in Gwangyang
4. For coating weight of Cr film and Organic film, additional agreement is required